(english) The intensity of deformation at a point in an object. See normal strain and shear strain.
(english) In two dimensions, a fixed support restrains three degrees of freedom: two translations and one rotation.
(Environmental Engineering) Water which is contained in geologic strata. Also properly written as two words, ground water.
(english) The ratio of shear stress divided by the corresponding shear strain in a linear elastic material.
(english) Forcing metal to flow in a direction opposite to the motion of a punch or die.
(Concrete Engineering) The water in concrete which is irremovable by oven drying; chemically combined during cement hydration.
(english) Joining metals by fusion of nonferrous alloys that have melting points above 800 F (425C), but lower than those of the metals being joined. May be accomplished by a torch. Filler metal is ordinarily in rod form in torch brazing; whereas in furnace and dip brazing the work material is first assembled and the filler metal may then be applied as wire, washers, clips, bands, or may be bonded, as in brazing sheet.
(Concrete Engineering) A device used in determining time of setting of hydraulic cement, described in ASTM 0 266. Gradation The sizing of granular materials; for concrete materials, usually expressed in terms of cumulative percentages larger or smaller than each of a series of sieve openings or the percentages between certain ranges of sieve openings.
(Environmental Engineering) A unit of varying dimensions in a landfill which is isolated from the environment by 6 to 12 inches of soil cover. A cell is one day's waste or less. A cell is covered with soil at the end of each day.
(english) A coating defect consisting of a lower coating film weight on the bottom of the coated sheet caused by high velocity air in the oven. Blow back usually occurs with high solids coatings which have little solvent to evaporate and "set" the film.
(english) A steel making process wherein oxygen of the highest purity is blown onto the surface of a bath of molten iron contained in a basic lined and ladle shaped vessel. The melting cycle duration is extremely short with quality comparable to Open Hearth Steel.
(Concrete Engineering) Concrete panels, usually architectural designs, reinforced with a high zirconia (16% minimum), alkali-resistant glass fiber. Optimum glass fiber content of 5% by weight. Lower fiber content results in lower early ultimate strengths, higher fiber content can produce composite compaction and consolidation difficulties.